硬质pvc透明包装薄膜的生产工艺流程与生产工艺是怎样

2025年09月07日 09:11:03      来源:雄县绝缘材料厂 >> 进入该公司展台      阅读量:9

分享:

(1)出产工艺流程。硬质PVC包装膜出产工艺流程如下。种种质料→捏合→冷拌跟→挤出吹塑→PVC玻璃纸基膜→抗静电、热封涂覆处置→分切→测验→包装→制品本工艺流程采取粉料直接挤出吹塑成型,制成玻璃纸基膜后,亦可直接作为制品,而不经抗静电、热封涂覆处置。
(2)出产工艺。硬质PVC通明包装膜个别采取挤出上吹成型工艺,重要工艺前提先容如下。①配料捏合。将PVC树脂及其余助剂按配朴直确称量后,放入高速捏合机,捏适时光5~8min,温度102℃左右,物料捏合好后放入冷却器停止冷却,待物料温度落到40-50℃以下即可放
1 production process. RIGID PVC packaging film production process is as follows. Seed Material → kneading → cold mixing → extrusion blow molding → PVC cellophane base film → antistatic, heat sealing coating → cutting → testing → packaging → product direct extrusion blow molding, made of Cellophane base film, can also be directly used as products, without anti-static, heat sealing coating disposal. 2 production process. RIGID PVC transparent packaging film individual to adopt extrusion blow molding process, the important process premise as follows. 1 Ingredient kneading. The PVC resin and other auxiliaries are weighed accurately according to the match plain, put them into high-speed kneading machine, kneading time is 5 ~ 8 minutes, the temperature is about 102 °C, after kneading the materials, put them into the cooler to stop cooling, wait for the temperature of the materials to fall below 40-50 °C

版权与免责声明:
1.凡本网注明"来源:全球工厂网"的所有作品,版权均属于全球工厂网,转载请必须注明全球工厂网。违反者本网将追究相关法律责任。
2.企业发布的公司新闻、技术文章、资料下载等内容,如涉及侵权、违规遭投诉的,一律由发布企业自行承担责任,本网有权删除内容并追溯责任。
3.本网转载并注明自其它来源的作品,目的在于传递更多信息,并不代表本网赞同其观点或证实其内容的真实性,不承担此类作品侵权行为的直接责任及连带责任。其他媒体、网站或个人从本网转载时,必须保留本网注明的作品来源,并自负版权等法律责任。 4.如涉及作品内容、版权等问题,请在作品发表之日起一周内与本网联系。