![](https://img70.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5d09c556a05fdb68c1c2c9160aa2ac180.jpg)
![](https://img70.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5700086a37a872f5b62e01ef5e0c023d1.jpg)
![](https://img65.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5805c61a8e1b6af590adb364492b436c3.jpg)
![](https://img65.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5b3f1187b9b9668e18568569101e8b923.jpg)
![](https://img65.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb594a5654d3fc3a72402709195f3dc100b.jpg)
![](https://img65.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5b055b934ef912c56a0ef23fb02dbd142.jpg)
![](https://img65.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb550efe5de78885ec366dc047bbff9c3be.jpg)
![](https://img61.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5a3d6b7f3602c41b4e98715103d11f1e4.jpg)
![](https://img69.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5591ba190abc67ab630dc097512cde9af.jpg)
![](https://img69.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb504c5c31ffe8c90f53c9ba05fc8e253af.jpg)
![](https://img69.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb508e9336a8b8409e9451a4f5b1ae8d4e1.jpg)
![](https://img69.gc1288.com/5eceadd4559dcfd2f3a66a21be9a899b03db066b6cc84bb5585e927ab4a5ff3e1e932fcd96ae93ea.jpg)
42CrMo钢:是超高强度钢,具有高强度和韧性,淬透性也较好,无明显的回火脆性,淬火时变形小,调质处理后有较高的疲劳极限和抗多次冲击能力,低温冲击韧度良好,高温时有高的蠕变强度和持久强度,及可靠的耐磨性。/r
/r
/r
45钢:调质处理后零件具有良好的综合机械性能,广泛应用于各种重要的结构零件,特别是那些在交变负荷下工作的连杆、螺栓、齿轮及轴类等。但表面硬度较低,不耐磨。可用调质+表面淬火提高零件表面硬度。/r
/r
/r
42CrMo与45钢区别/r
/r
1: 42CrMo 为合金结构钢,碳含量为0.38--0.45%,含铬0.9--1.2%,含钼0.15--0.25%,抗拉强度为1100MPa ,屈服点为950MPa 。用负荷较大,耐磨性好!要求可靠性较高的零部件。/r
/r
/r
2: 45为优质碳素结构钢,碳含量为0.42--0.50%,抗拉强度为610MPa ,屈服点为360MPa ;用于一般轴类零件。